We are regularly making the following Steel grades:
MS round bars, En8 round bars, En8D round bars, SAE 1018 round bars, SAE 1008 round bars, SAE 1010 round bars, IS 2062 round bars, A105 round bars, LF2 round bars, EN19/SAE 4140 round bars, EN24 round bars, EN31 round bars, SAE 52100 round bars, 20MnCr5 round bars, EN1A round bars, EN9 round bars, C15, C20, C25, C22, C30, SS etc.
Steel Round bar sizes in mm
16,18,20,21,22,24,25,26,27,28,30,32,34,36,37,38,40,42,44,47,50,53,56,60,63,65,71,75,80,85,90,100,110,120,125,130 mm |
Round Corner Square (RCS) or Rolled billet sizes in mm
65x65,75x75,90x90,100x100,115x115,115x125 |
Square Sharp cornered bar sizes in mm
40x40,42x42,50x50,53x53 |
Hex bar sizes in mm
24, 27.5, 28.5, 29.5, 32, 34, 38, 40, 43, 48, 53, 57, 63 |
MS / SS Flat Bars |
MS / SS Angle |
MS Channel
|
Bright Bars
| Round |
: |
14 mm to 76 mm dia |
| Square |
: |
25 mm to 50 mm |
| Hex |
: |
22 mm to 60 mm |
| Tolerance : |
Black Bar |
As per IS-3739 grd II std |
|
Bright Bar |
As per ISO H8, H9, H10, H11 also as
per ASTM A484, DIN 17440, 671 or
as per mutual agreement. |
| |
|
|
| Length: |
Black Bar |
3 to 6 meters +0.1 mtr |
|
Bright Bar |
3 to 6 meters +0.1 mtr tolerance or
as per Customer's Requirement |
| |
|
|
| Straightness: |
Black Bar |
5mm / mtr. |
|
Bright Bar |
< 1 mm / mtr or as per Mutual agreement |
| |
|
|
Mechanical
Properties : |
Black Bar |
As per ASTM or DIN |
|
Bright Bar |
ASTM, DIN or As mutually agreed upon. |
| |
|
|
Delivery
Condition : |
Black Bar |
Hot Rolled - Straightened
Hot Rolled - Annealed - Straightened
Hot Rolled - Soln. Ann. - Straightened |
| |
Bright Bar |
Drawn - Polished
Drawn - ground - polished
Peeled - Polish
Peeled - ground - polished |
| Grades |
| Classification |
IS |
EN |
DIN |
AISI/SAE |
|
| Mild Steel |
IS : 2062, 2830, 2831, 15C8, 20C8, 25C8, CL-I, CL-II |
EN-3B, EN-32B |
CK-15, CK-20, CK-25 |
1008, 1010, 1015, 1018, 1020, 1025 |
|
| Medium Carbon Steel |
30C8, 35C8, 40C8, 45C8, 50C8, 55C8, CL-III, CL-IV, CL-V |
EN-8, EN-8D, EN-9 |
CK-30, CK-35, CK-40, CK-45, CK-50, CK-55, CK-60 |
1030, 1035, 1040, 1045,1050, 1055, 1060 |
|
| |
| Grades - Alloy Steel Round Bars |
| Popular Grades offered for Round Bars under the Alloy Steel category are as follows |
| Internal Standard |
Equivalent Grades |
BS |
DIN |
IS |
EN |
SAE/AISI |
| EN18 |
530A40 |
37Cr4 |
40Cr1 |
EN18 |
5140 |
| EN24 |
817M40 |
34CrNiMo6 |
40NiCr4Mo3 |
EN24 |
4340 |
| EN19C |
709M40 |
- |
40Cr4Mo3 |
EN19C |
4140, 4142 |
| EN19 |
709M40 |
- |
40Cr4Mo3 |
EN19 |
4140, 4142 |
| EN18D |
530A40 |
37Cr4 |
40Cr1 |
EN18D |
5140 |
| EN18C |
530A40 |
37Cr4 |
40Cr1 |
EN18C |
5140 |
| EN18A |
530A40 |
37Cr4 |
40Cr1 |
EN18A |
5140 |
| 27C15 |
- |
28Mn6 |
27C15 |
- |
1527 |
| 20MnCr5 |
- |
20MnCr5 |
20MnCr1 |
- |
- |
| 20Mn2 |
150M28 |
- |
20Mn2 |
EN14A |
1524 |
| 16MnCr5 |
- |
16MnCr5 |
17Mn1Cr95 |
- |
5120 |
| EN18B |
530A40 |
37Cr4 |
40Cr1 |
EN18B |
5140 |
| SAE8620 |
805M20 |
- |
20NiCrMo2 |
EN362 |
8620 |
| SAE8622 |
805M20 |
- |
20Ni2Cr2Mo2 |
- |
8622 |
| EN353 |
815M17 |
- |
15NiCr1Mo12 |
EN353 |
- |
| EN354 |
820M17 |
- |
15NIVCr1Mo15 |
EN354 |
4320 |
| 15Cr3 |
523A14 |
15Cr3 |
15Cr65 |
EN206 |
5015 |
| EN24 |
817M40 |
34CrNiMo6 |
40NiCr4Mo3 |
EN24 |
4340 |
| 17Cr3 |
- |
17Cr3 |
- |
- |
- |
| 40Cr4 |
41Cr4 |
41Cr4 |
40Cr4 |
En18D |
5140 |
| 34Cr4 |
34Cr4 |
34Cr4 |
- |
En18 |
5130 |
| Grades - Carbon Steel Round Bars |
| Some of the popular grades offered for Round Bars under the Carbon Steel category are as follows |
| Internal Standard |
Equivalent Grades |
BS |
DIN |
IS |
EN |
SAE/AISI |
| EN15B |
150M36 |
36Mn5 |
37Mn2, 37C15 |
EN15B |
1536 |
| EN32B |
- |
CK15 |
C14 |
EN32B |
1015,1016,1018 |
| 1038 |
- |
CK38 |
- |
- |
1038 |
| EN43C |
- |
- |
C50 |
EN43C |
1050 |
| CK45 |
- |
CK45 |
45C8 |
1045 |
- |
| EN9 |
070M55 |
CK55 |
C55 |
EN9 |
1055 |
| C35 |
- |
C35 |
35C8 , C35Mn75 |
- |
1035 |
| EN42 |
- |
CK75 |
80C6 |
EN42 |
1074 |
| EN42B |
- |
C67 |
65C6 |
EN42B |
1065 |
| EN43 |
080M50 |
C55 |
60C6 |
EN43 |
1055 |
| EN43B |
080A47 |
CK45 |
- |
EN43B |
1045 |
| EN8 |
|
|
|
|
|
| |
| Grades - Low Carbon Steel Round Bars |
| Some of the popular grades offered for Round Bars under the Low Carbon Steel category are as follows |
| Internal Standard |
Equivalent Grades |
DIN |
IS |
EN |
SAE/AISI
|
| SAE 1008 |
- |
- |
- |
- |
| SAE 1010 |
CK10 |
C10 |
- |
SAE1010 |
| SAE 1018 |
CK15 |
C15Mn75 |
EN32B, EN32C |
SAE1018 |
|