We are one of the top Stainless Steel 304 Bright Round Bar manufacturers in Gujarat and manufacture a vast range of sizes from best quality billets and ingots. The range of products of SS 304 Bright Round Bar which we offer to our customers are of export quality and we are exporting to all major countries. These ASTM 276 AISI 304 Stainless Steel Bright Round bars have been made keeping in mind the quality parameters which have been set by the industry and we offer H9 and H11 tolerance. We do testing like Ultrasonic test, visual inspection, mpi and pmi of each and every piece and because of this we don’t get any quality complaints from our customers. Our customers prefer our products over all our competitors because of these reasons. We offer standard as well as custom and fixed length as per customer requirements.
Stainless Steel 304 Bright Round Bars are always supplied with the test certificates and can be supplied in bulk quantity as well as retail quantity as per customers requirements. SS 304 export bright round bars are supplied by us to various industries and we are also offering wholesale quantity at discounted prices. We are making black bars as well as SS 304 Round bright bars and 304 SS export bright bars.
SS 304 rods are non magnetic, Corrosion resistant and have good machinability, good weldability, and high strength and impact properties in either normalized or hot rolled condition.
SS 304 Bright Chemical Composition:
| Element | Content |
|---|---|
| Carbon, C | 0.080 max % |
| Manganese, Mn | 2.0 % |
| Chrome, Cr | 18 – 20 % |
| Nickel, Ni | 8.0 – 10.50 % |
| Phosphorous, P | 0.045 % |
| Sulfur, S | 0.030 % |



Our Size Range Of SS Bright 304 Round Steel Bars:
16mm, 17mm, 18mm, 20mm, 21mm, 22mm, 23.5mm, 24mm, 25mm, 26mm, 27mm, 28mm, 30mm, 32mm, 34mm, 35mm, 36mm, 37mm, 38mm, 40mm, 42mm, 45mm, 46.5mm, 47mm, 50mm, 51mm,53mm, 56mm, 60mm, 63mm, 65mm, 70mm, 75mm, 78mm, 80mm, 85mm, 90mm, 95mm, 100mm, 105mm, 110mm, 115mm, 120mm, 125mm, 130mm.
Grades We Manufacture in addition to SS 304 Export Bright Round Bars:
SS 410, SS 202, SS 304, SS 316, SS 420, MS, SAE 1018, IS 2062, A105, 1008, SAE 1010, SAE 1015, C15, C18, C20, 1020, C22, 1022, C25, 1025, SS 202, 1030, C35, 1035, 35C8, S35C, C40, 1040, C45, 45C8, 1045, CK45, C50, 1050, C55, 55C8, 1055, C60, 1060, C70, 41Cr4, 40Cr4, 40Cr1, En18, En18D, SAE 1541, SAE 1536, 37Mn2, 37C15, En15, SAE 1141, LF2, EN19, SAE 4140, 42CrMo4, EN24, EN31, SAE 52100, 20MnCr5, 8620, EN1A, EN8, EN8D, EN9, ST 52.3, EN42, En353 and other grades as per customer requirement.
Cities to which we supply SS 304 Steel Round Bars:
Ahmedabad, Surat, Baroda, Kadi, Rajkot, Surendranagar, Mumbai, Pune, Chakan, Bhosari, Ranjangaon, Aurangabad, Ahmednagar, Kolhapur, Belgaum, Thane, Nagpur, Nashik, Chennai, Jaipur, Indore, Ajmer, Hyderabad, Hubli, Karnataka, Gujarat, Maharashtra, Rajasthan, Madhya Pradesh and other parts of India. We have SS 304 Steel Round Bar Stockists, Supplier, Wholesaler, Distributor, Dealer, Traders all over India.
Certifications:
We are ISO 9001:2015 certified and we also have IS 2062 license from Bureau of Indian Standards for steel rounds for use in various structural, bright bars and other engineering applications. In addition to that we also have BIS certification to manufacture rounds for boilers.