EN24 Round Bars, EN24 Round Bar manufacturer, EN24 Rods Supplier, Dealer, Stockists
We are EN24 Round Bar manufacturers and we are only manufacturing from prime quality billets and blooms. The range of EN24 Round Bars which we manufacture for our customers are of high quality and these round bars are used for making machineries and OEM Auto components. These products have been made keeping in mind the quality parameters which have been set by the industry in the market. EN24 Round Bars are always supplied with the test certificates and can be supplied in bulk quantity as well as retail quantity as per customers requirements. EN24 alloy Steel round bars are supplied by us to various industries.
EN24 is a very high strength steel alloy which is hardened and tempered before supplying and has nickel, chromium, molybdenum making it high tensile steel strength, with good ductility and wear resistance. With relatively good impact properties at low temperatures, EN24 is also suitable for a variety of elevated temperature applications. EN24 round bars have good internal strength and high external strength, which makes it highly wear resistant. EN24 steel round bars offer good combination of ductility, strength and wear resistance. En24 is a very high strength alloy engineering steel.
Equivalent grades of EN24 round bars
SAE/AISI 4340
34CrNiMo6
BS 817M40
IS 40NiCr4Mo3
Chemical Composition of SAE EN24 round bars
| Carbon | 0.36 - 0.44 |
| Manganese | 0.45 - 0.70 |
| Silicon | 0.10 - 0.35 |
| Sulfur | Max 0.040 |
| Phosphorus | Max 0.035 |
| Chromium | 1.00 - 1.40 |
| Molybdenum | 0.20 - 0.35 |
| Nickel | 1.30 - 1.70 |
Our Size Range Of EN24 Round Steel Bars
16mm, 18mm, 20mm, 22mm, 23.5mm, 24mm, 25mm, 26mm, 27mm, 28mm, 30mm, 32mm, 34mm, 35mm, 36mm, 37mm, 38mm, 40mm, 42mm, 45mm, 46.5mm, 47mm, 50mm, 51mm,53mm, 56mm, 60mm, 63mm, 65mm, 70mm, 75mm, 78mm, 80mm, 85mm, 90mm, 95mm, 100mm, 105mm, 110mm, 115mm, 120mm, 125mm, 130mm.
Grades We Manufacture in addition to EN24 Round Bars
MS, SAE 1018, IS 2062, A-105, SAE 1008, SAE 1010, SAE 1015, C15, C18, C20, 1020, C22, 1022, C25, 1025, C30, 1030, C35, 1035, 35C8, S35C, C40, 1040, C45, 45C8, 1045, CK45, C50, 1050, C55, 55C8, 1055, C60, 1060, C70, 41Cr4, 40Cr4, 40Cr1, En18, En18D, SAE 1541, SAE 1536, 37Mn2, 37C15, En15, SAE 1141, LF2, EN19, SAE 4140, 42CrMo4, EN24, EN31, SAE 52100, 20MnCr5, 8620, EN1A, En8, 4140D, EN9, ST 52.3, EN42, En353, SS 410, SS 202, SS 304, SS 316 and other grades as per customer requirement.
Cities to which we supply EN24 Steel Round Bars
Ahmedabad, Surat, Baroda, Kadi, Rajkot, Surendranagar, Mumbai, Pune, Chakan, Bhosari, Ranjangaon, Aurangabad, Ahmednagar, Kolhapur, Belgaum, Thane, Nagpur, Nashik, Chennai, Jaipur, Indore, Ajmer, Hyderabad, Hubli, Karnataka, Gujarat, Maharashtra, Rajasthan, Madhya Pradesh and other parts of India.
Certifications for EN24 Round Bars
We are ISO 9001 certified. We also have IS2062 license of Bureau of Indian Standards for steel rounds for use in various structural, bright bars and other engineering applications. We also have BIS certification to manufacture rounds for boilers.