Kadi, Mehsana, Gujarat: 382715

Give Us a Call

Our Number: +91-9712932024

Email Us

bsapl@kanoigroup.com

Contact us for your requirement of Carbon Steel Round bars and Alloy Steel Round Bars. MS, SAE 1018, IS 2062, A-105, SAE 1008, SAE 1010, SAE 1015, C15, C18, C20, 1020, C22, 1022, C25, 1025, C30, 1030, C35, 1035, 35C8, S35C, C40, 1040, C45, 45C8, 1045, CK45, C50, 1050, C55, 55C8, 1055, C60, 1060, C70, 41Cr4, 40Cr4, 40Cr1, En18, En18D, SAE 1541, SAE 1536, 37Mn2, 37C15, En15, SAE 1141, LF2, EN19, SAE 4140, 42CrMo4, EN24, EN31, SAE 52100, 20MnCr5, 8620, EN1A, EN8, EN8D, EN9, ST 52.3, EN42, En353, SS 410, SS 202, SS 304, SS 316 and other grades as per customer requirement.