C30 Round Bars, C30 steel round bars manufacturer supplying to Stockists, Supplier, trader, dealer, wholesaler, distributor
We are C30 Round Bar manufacturers and manufacture a vast range of sizes and use only from prime quality billets and blooms as raw material. The range of products of C30 Round Bar which we offer to our customers are of high quality and these round bars are used for making machineries and OEM Auto components. These products have been made keeping in mind the quality parameters which have been set by the industry in the market. C30 Steel Round Bars are always supplied with the test certificates and can be supplied in bulk quantity as well as retail quantity as per customers requirements. C30 round bars are supplied by us to various engineering and forging industries and used in Levers, Bolts, Nuts, Studs.
AISI C30 steel is a medium tensile steel supplied in the black hot rolled or normalized condition. It has Brinell hardness ranging between 170 and 210 and tensile strength of 570 - 700 MPa. AISI C30 steel has good machinability, good weldability, and high strength and impact properties in either the normalized or hot rolled condition. SAE C30 steel has a low through-hardening capability with only sections of size around 60 mm being recommended as suitable for tempering and through-hardening. However, it can be efficiently flame or induction hardened in the normalized or hot rolled condition to obtain surface hardnesses in the range of Rc 54 - Rc 60 based on factors such as section size, type of set up, quenching medium used etc.
AISI C30 Chemical Composition:
| Element | Content |
|---|---|
| Carbon, C | 0.270 - 0.340 % |
| Iron, Fe | 98.63 - 99.09 % |
| Manganese, Mn | 0.60 - 0.90 % |
| Phosphorous, P | 0.040 % |
| Sulfur, S | 0.050 % |
Equivalent grades of C30 round bars:
EN Name C30 (1.0501)
EN Number 1.0501
DIN C30, CM30
BS 970 070M36
UNI C30
JIS S30C
Our Size Range Of C30 Round Steel Bars:
16mm, 18mm, 20mm, 22mm, 23.5mm, 24mm, 25mm, 26mm, 27mm, 28mm, 30mm, 32mm, 34mm, 35mm, 36mm, 37mm, 38mm, 40mm, 42mm, 45mm, 46.5mm, 47mm, 50mm, 51mm,53mm, 56mm, 60mm, 63mm, 65mm, 70mm, 75mm, 78mm, 80mm, 85mm, 90mm, 95mm, 100mm, 105mm, 110mm, 115mm, 120mm, 125mm, 130mm.
Grades We Manufacture in addition to C30 Round Bars:
MS, SAE 1018, IS 2062, A105, 1008, SAE 1010, SAE 1015, C15, C18, C20, 1020, C22, 1022, C25, 1025, C30, 1030, C35, 1035, 35C8, S35C, C40, 1040, C45, 45C8, 1045, CK45, C50, 1050, C55, 55C8, 1055, C60, 1060, C70, 41Cr4, 40Cr4, 40Cr1, En18, En18D, SAE 1541, SAE 1536, 37Mn2, 37C15, En15, SAE 1141, LF2, EN19, SAE 4140, 42CrMo4, EN24, EN31, SAE 52100, 20MnCr5, 8620, EN1A, EN8, EN8D, EN9, ST 52.3, EN42, En353, SS 410, SS 202, SS 304, SS 316 and other grades as per customer requirement.
Cities to which we supply C30 Steel Round Bars:
Ahmedabad, Surat, Baroda, Kadi, Rajkot, Surendranagar, Mumbai, Pune, Chakan, Bhosari, Ranjangaon, Aurangabad, Ahmednagar, Kolhapur, Belgaum, Thane, Nagpur, Nashik, Chennai, Jaipur, Indore, Ajmer, Hyderabad, Hubli, Karnataka, Gujarat, Maharashtra, Rajasthan, Madhya Pradesh and other parts of India. We have C30 Steel Round Bar Stockists, Supplier, Wholesaler, Distributor, Dealer, Traders all over India.
Certifications:
We are ISO 9001 certified. We also have IS2062 license of Bureau of Indian Standards for steel rounds for use in various structural, bright bars and other engineering applications. We also have BIS certification to manufacture rounds for boilers.